Roofing Slate Inspection Checklist: What to Check When the Container Opens

The sixty-second version: when a container of roofing slate arrives, most of the damage is already done — or already visible. Start with the container and its seal, check the packing slip against your order, then open a first crate and run the five checks: colour, size, thickness, edges, and the ring test. Compare breakage against the allowance written into your contract, photograph everything that's broken, and keep the paperwork — because a clean roof starts with what you catch at the gate, not on the roof.

Part of the Roofing Slate Guide's Quality, Testing & Standards section. This is the receiving end of the story: our test-report walk-through decodes the paper, and this page is what you do when the paper and the pallets finally meet at your door.

When the container door opens on delivery day, the instinct is to pull the first crate open and see the colour, run a hand over the surface, and start planning the roof. It's also the most expensive instinct in the whole slate trade, because the evidence doesn't wait. The moment the crates hit the forklift, the batch mix-ups scatter and a handling failure stops being provable. You can't count a batch that's already stacked three high, and you can't photograph a tipped crate after it's been turned twice. So this page is not a list of things to check someday — it's the exact order to run them in, with the figures to judge them against, in the first hour after the door opens.

The checks below are written the way roofing slate is actually made, inspected and shipped out of a factory, and they're meant to hold up when an importer, a roofing contractor or a buyer's inspector works through them. Two things to keep in mind the whole way through: natural roofing slate is not a CNC-machined product, and the figures that count are the ones agreed with your supplier — not a universal default.

Slate crates being unloaded from a container while a warehouse worker records the delivery inspection on a clipboard
The inspection starts at the container door, not the roof — a photograph with the crate number in frame is the evidence that settles most questions.

Before you touch a tile: the paperwork check

Everything else on this page is about the stone. But the stone check only makes sense if the stone matches the paper. So the first ten minutes go to paperwork, and it's done in this exact order:

  • 1. The packing slip vs. the purchase order. Size, colour, thickness, quantity, grade — five numbers. If the slip says 500×250 and you ordered 500×250, good. If it says something else, stop and call the supplier before you open anything. This is the cheapest moment to catch a problem.
  • 2. The test report and batch number. You read the test report when you bought the stone. Now check the batch number on the report against the batch number on the packing list and on the crates themselves. It should be the same number three times. If it isn't — if the paper describes batch A and the crate says batch B — the report is describing someone else's slate, and that's a conversation to have before the container is unloaded.
  • 3. The crate count. The slip says 400 crates, 8 pallets per pack, 5,000 tiles. Count the crates while they're still stacked. It takes two minutes and it's the one check that can't be undone after.

That's the paperwork pass. It's boring, and it's the highest-value five minutes in the whole delivery. Because the second the fork truck starts moving crates, the "which batch was where" information is lost forever.

The container and the seal: the minutes before the door opens

The inspection actually starts at the container itself, not the first crate — because there are two things you can only evidence once, and they're both outside the crates. Work through them before the door is fully open:

  • 1. The container and seal numbers. Check the container number and the seal number on the container against the transport documents, and photograph the seal before it's cut. If the seal number doesn't match the paperwork, stop and note it — that's a question for the carrier, not for the cargo.
  • 2. Photograph the exterior first. The door, the seal, and any dents, torn panels or scuffed edges. The outside of the container tells you the first thing about what the load went through, and it can't be staged later.
  • 3. Open the door safely. Stand clear of the opening and open against the door, in case cargo has shifted and settled against it. No one stands in front of the first pull — a shifted crate can fall when the door releases.
  • 4. Check the crates before you touch one. Look for crates that are tipped, tilted, wet or visibly damaged. A tipped crate changes how you read its breakage later, and wet packaging needs its own record.
  • 5. Keep the transport paperwork. The bill of lading, the delivery note and any exception the driver signs all belong in the same folder as your photos.

None of this needs a specialist — it's five minutes that decide whether the "was it like this when it arrived" conversation is a matter of fact or a matter of guesswork.

Then open a crate: the ten-minute visual pass

Not all of them. For the first pass, open one crate from the middle of the stack, not the easiest one on top — that's the one that's been handled most and shows it. Cut the straps, pull the lid, and work through the tile checks in this order. Then remember that one crate is only a first read: for a full acceptance, sample across different crates and different positions in the stack — top, middle, bottom, back — because batch and colour variation, and handling damage, don't sit in a single crate.

CheckWhat you're looking atFail if…
Colour & batchAre the tiles the colour you approved? Are there two visibly different batches in the same crate?Two tones in one crate, or the colour doesn't match your approved sample.
SizeTake a tile and measure length, width and thickness with a calliper.Outside the tolerance you agreed with the supplier (see the thickness section below).
EdgesRun a thumbnail along each edge. Look for chips, crumbling, or edge lift.Chipped edges on more than a small share of the tiles, or any edge that crumbles under a fingernail.
Ring testHold a tile by the corner and tap it lightly with a steel trowel or hammer handle.A dull thud instead of a clean ring — a sign to look closer at that tile (edge, crack, delamination).
SurfaceLook for pyrite spots, carbonate ribbons, rust streaks, or a waxy surface.Visible pyrite that catches light, soft carbonate bands, or a sheen that says the surface was waxed to hide flaws.

The ring test is the one the roofers all know and nobody writes down, so give it the right weight. It's a useful on-site screening method, not a verdict on its own. Hold a tile by a corner and tap it lightly with a steel trowel or hammer handle; clean slate rings like a bell, and a cracked or delaminating tile gives a dull, dead thud. You don't need perfect pitch — you need the difference between "ring" and "thud". But the sound is affected by the tile's size, thickness, how it's supported and where you tap, so a single dull tone tells you to look closer at that tile (an edge, a hairline, a light band), and a cluster of dull thuds across several crates is a reason to widen your sample and check further — it's a signal to investigate, not a standalone verdict that rejects the batch by itself.

The thickness check: where the numbers meet the spec

Thickness is the single dimension that changes everything else about a roof — the weight, the fixing, the headlap, the coverage. And it's the one most sloppy deliveries fail on. Measure at least five tiles from your sample crate, at each of the four edges, and note the spread. Then check that spread against what was agreed, not against a default number in anyone's memory.

Natural roofing slate is not a CNC-machined product, so its thickness variation has to be read against the agreed product specification, the manufacturing method and the applicable standard, rather than a single universal tolerance. As a practical reference for the two main surface types:

Slate surfaceRealistic thickness spreadWhy it matters
CNC-dressedaround ±0.5 mm, where the order spec matches the processRoof weight and fixing stay predictable — but only if your agreed spec says so.
Hand-split / naturally cleftvaries with grade and order, often ±1 mm or moreCharacterful, but the roof gets a mix — confirm the spread against the order, don't assume it.

And the rule that catches more bad loads than any other: write down the thickness you find, then check it against the thickness on the packing slip. If the slip says 6 mm and your calliper reads 4.8 mm on the average, that's not a tolerance question — it's a different product. Keep the calliper out for the next check.

Digital caliper measuring the edge thickness of a roofing slate tile
A calliper across the edge closes the loop on the packing slip — measure several tiles, note the spread, and compare it to what you ordered.

The four defects you can't un-see

There's a short list of defects that are — to borrow a phrase from the roofing trade — "deal-breakers" on inspection. Not every flaw kills a slate; some are cosmetic. These four change the performance of the tile, and they're worth knowing by name:

  • 1. Delamination — the slate's layers have started to separate. You'll see it as a light-coloured edge or a flaky corner. It means the tile will peel like a book over years. Delamination is a full reject.
  • 2. Pyrite spots — small gold or iron-coloured dots that oxidise, swell, and eventually pop small pits out of the face. Some is normal; a face full of them is a waiting façade problem.
  • 3. Carbonate ribbons — soft, light-coloured bands that run through the stone. They look pretty and they're a trap: they erode faster than the slate around them, and in a wet climate they'll be the first thing to go. It's the same story we told in the carbonate explainer.
  • 4. Edge chipping — a broken corner or a nib that's already gone. A couple of chips are normal in transport. When they're everywhere, your handling is at fault, or the packaging was too rough.
Gloved fingers inspecting a flaking delaminated edge on a roofing slate tile
A light-coloured, flaking edge is the classic delamination read — the layers are starting to separate, and the tile will keep peeling over years.

Here's the honest part about breakage: a certain amount of breakage is built into the deal. It moves in a container, it gets strapped, it gets lifted. A responsible importer budgets for it. The word "breakage" is not a four-letter word; the word "unchecked" is. Your job at the gate is to photograph it, count it, and agree with the driver that it's there — then you and the supplier work out whether it's within the agreed allowance or not. Photograph every cracked tile where it is, from two angles, with a reference to the crate number. If you do nothing else, do this: a picture of the broken tile on the dock is worth ten emails.

The breakage allowance: a number to write down

What's realistic? In practice, most reputable suppliers and buyers agree on a breakage allowance when they sign — commonly in the range of 1–3% of the shipment, the crunched corners and snapped tiles that normal container motion produces. The number that counts is the one in your contract, not an average guessed at the dock. When you see a single crate that's 15% broken, that's not an allowance — that's a handling failure, either the straps were too tight, the crate was stacked upside down, or the container was dropped. There is a whole section of the buying guide on this, but the inspection version is: the average matters, and the outlier matters more. Photograph the outlier.

Also worth knowing before you open the crate: some suppliers mark the expected breakage on the packing or in their terms. If they don't, ask for the allowance in writing before you sign — the buyer who asks "what's your allowance?" before the order is placed has already done half the inspection.

The ten-minute close: when to reject, when to accept

At the end of the visual pass, you have enough to make a call. And the call is rarely a black-and-white "reject everything" — it's more often a shade of grey, and the professional move is to have a grading rule ready. Here's a workable one:

FindingAction
Slip doesn't match order (size, colour, thickness, quantity)Stop. Don't unload. Email the supplier with the photo before you break anything else.
Ring test thuds on a large share of one crate (e.g. >10%)Hold, don't reject yet. Widen the sample across more crates and re-check — a high thud rate is a signal to investigate, not a verdict on the whole batch. Photograph the evidence.
Thickness spread beyond the agreed tolerancePause. Re-measure ten tiles across different crates before you decide. This is where the calliper saves your roof.
Breakage within the contracted allowanceAccept, but photograph everything and sign the packing slip with a note.
Colour is consistent, tiles ring, edges are goodAccept, and stack the crates so the good ones go on the roof first.

One phrase to keep in mind, because every inspector eventually says it to a client: "You can't reject a broken tile after it's been unloaded." What that means is practical, not legal absolute: whether a breakage can be claimed depends on your transport terms, your contract, your insurance and the applicable law — so the safe play is to record, photograph and notify the supplier within the deadline your documents allow. The inspection is where the evidence is cleanest, and that's where the question is settled.

The incoming inspection record: fill it in on the dock

Every read in the checklists above is worth more when it's written down. This is the sheet to carry to the dock and fill in for each delivery — it turns the routine into a record that stands up in a claim:

Roofing Slate Incoming Inspection Record

Container / seal No.______
Purchase order / batch No.______
Crates received______
Crates sampled______
Tile dimensions (L × W)______
Thickness range______
Visible damage count______
Inspection photos (crate refs)______
DecisionAccept / Hold / Reject

Keep one sheet per delivery, with the photos, in the same folder as the transport documents. It's the smallest record that decides the next hour — and the next invoice.

The 1-page checklist you can print

Here's the whole thing, condensed to one sheet, in the order to run it. Copy this into your delivery-day folder, screenshot it to your phone, or pin it to the site office wall:

Roofing Slate Delivery Checklist — one page

  1. Paperwork first — packing slip vs PO: size, colour, thickness, quantity.
  2. Batch match — report batch = packing batch = crate batch. Three matches or stop.
  3. Container & seal — check and photograph the seal number before it's cut.
  4. Open the door safely — clear of the opening, watch for shifted cargo.
  5. Count the crates — on the dock, before the fork truck.
  6. Open a first crate from the middle; sample across different crates for full acceptance.
  7. Five-tile pass — colour, size, edges, ring test, surface.
  8. Thickness with a calliper — 4 edges, 5 tiles, note the spread vs the spec.
  9. Four defects — delamination, pyrite, carbonate ribbons, edge chips.
  10. Breakage — count it, photograph it, compare to the contracted allowance.
  11. Decide — accept / hold / reject, and write the decision down with the crate numbers.
  12. Photograph everything — a picture of the broken tile on the dock is your best document.

Photograph rule: two angles, a ruler for scale, the crate number in frame.

Factory worker inspecting a roofing slate tile for surface quality on the inspection bench before packing
Quality control begins where the slate is made — the same checks that protect a good delivery start on the factory bench, before the crate is ever sealed.

Frequently asked questions

How long does a roofing slate inspection take?

A proper one, on a normal delivery, is about an hour: 10 minutes of paperwork, 15 minutes of container and crate inspection, and 20–30 minutes of photographs and notes. The temptation is to race it — don't. An hour at the dock is cheaper than a week of arguing later.

What should I do if I find broken slates?

Photograph them from two angles with a reference (the crate number, a ruler), write down the count, and compare it to the breakage allowance written into your contract — commonly 1–3%. Then contact the supplier with the photos and the count, within the deadline your documents allow, and keep the broken tiles in a separate crate for the claim. The biggest mistake is to wash or stack them: the evidence disappears.

Is a crack in a slate always a reject?

Not every crack is a defect. Slate is split by hand, and a hairline that runs along the grain is often harmless, because the slate will follow that line when it's split anyway. But a crack across the grain, or one you can feel with a fingernail, changes the slate's strength. The ring test is the fast screen: if it still rings clean, it's usually usable; if it thuds, check the tile more closely and set it aside.

Can I inspect slate before the container reaches my warehouse?

Yes, and it's increasingly common. A pre-shipment inspection at the factory (by a third party, or with a video call) is cheaper and catches problems before the container is sealed. This checklist works the same there: the crate's still packed, the paperwork's the same, and the only difference is the roof is later. The factory inspection page in the buying guide covers the full routine.

What's the difference between inspection and test reports?

The test report is about the stone — what it will do over 40 years. The inspection is about the delivery — what you actually received today. They check different things: a test report says the stone is a certain water-absorption class; an inspection says the batch in this container is the right colour, the right size, and not over the contracted breakage. You need both, and they're both covered in the report page and this one.

Related Reading

Slate that arrives the way it left the factory

We run EN 12326 / ASTM C406 tested slate through CNC precision processing and individual inspection before it's packed — so the crate that opens at your door is the same stone that passed our bench. See the test results, browse the roofing slate range, or ask for samples before you commit.